Alloy Digest (1969) 18 (5): SA-239.
Published: 01 May 1969
... Unitemp 14 CMV is a low carbon, alloy steel recommended for welded structures operating at elevated temperatures up to 1100 F for short periods and at 1000 F for extended service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...