Alloy Digest (1970) 19 (8): Fe-44.
Published: 01 August 1970
... UNISEAL 42 is a closely controlled thermal expansion iron alloy used for glass-to-metal and metal-to-ceramic seals. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, joining...