Alloy Digest (1961) 10 (5): SA-114.
Published: 01 May 1961
... Unimach UCX-2 is essentially a 4100 type alloy with added cobalt and silicon. It can be heat treated to yield strengths of 225,000 to 235,000 psi. It has virtually no notch sensitivity. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...