Alloy Digest (1974) 23 (7): Fe-51.
Published: 01 July 1974
... UNILOY 888 is an iron-base, age-hardenable alloy designed primarily for applications requiring low magnetic permeability and high strength. It is austenitic at all times and its essentially non-magnetic characteristics are not impaired by various combinations of heat treatment and cold working...