Skip Nav Destination
Close Modal
Search Results for
Ultimo-200
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
Ultimo-200
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1968) 17 (8): SA-229.
Published: 01 August 1968
... ULTIMO-200 is a medium-carbon, chromium-molybdenum alloy steel capable of providing tensile strengths of over 200,000 psi in sections up to 4 inches diameter. It is recommended for heavy duty shafts, gears, rolls, bolts, etc. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
ULTIMO-200 is a medium-carbon, chromium-molybdenum alloy steel capable of providing tensile strengths of over 200,000 psi in sections up to 4 inches diameter. It is recommended for heavy duty shafts, gears, rolls, bolts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-229. Producer or source: Atlas Steels Company.
Journal Articles
Alloy Digest (1955) 4 (3): TS-31.
Published: 01 March 1955
... ULTIMO-6 is a chromium-nickel-molybdenum tool and die steel applicable where resistance to shock is important and where water cooling may be utilized with safety. It is particularly adapted to large dies where first cost is a major consideration. This datasheet provides information on composition...
Abstract
View article
PDF
ULTIMO-6 is a chromium-nickel-molybdenum tool and die steel applicable where resistance to shock is important and where water cooling may be utilized with safety. It is particularly adapted to large dies where first cost is a major consideration. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-31. Producer or source: Atlas Steels Company.