Journal Articles
Alloy Digest (1972) 21 (8): Ni-178.
Published: 01 August 1972
... UDIMET 80A is a precipitation-hardenable nickel-base alloy developed for elevated-temperature service. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance...