Alloy Digest (2020) 69 (8): TS-797.
Published: 01 August 2020
... Uddeholm Sverker 3 is a high-carbon, chromium-tungsten, alloy cold-work tool steel. It is suitable for medium and long run tooling in applications where a very good abrasive wear resistance is needed. Uddeholm Sverker 3 contains large carbides, which are advantageous for abrasive wear resistance...
Journal Articles
Alloy Digest (1979) 28 (11): TS-356.
Published: 01 November 1979
... AND ALLOYS @3-&iEE Inc. UHB SVERKER* 21 Upper Maotchtr. New Jay (Air-Hardening Cold-Work Steal; AISI Type 02) UHB WERKER 21 is a h&h-carbon, high+hromium cold-work tool steel alloyed with molybdenum and vanadium. It has high hardenability and high surface hardness after hardening. It has excellent wear...