Alloy Digest (1973) 22 (8): CS-52.
Published: 01 August 1973
... USS MACH-5 is a leaded resulfurized low-carbon steel containing bismuth. It is characterized by outstanding machinability, up to 50% better tool life, increased production and quality of machined parts, and up to 65% savings in job time. This datasheet provides information on composition, physical...