Alloy Digest (1970) 19 (12): SA-258.
Published: 01 December 1970
... USS FIFTY-N steel is a normalized high-strength low-alloy structural-quality plate steel having inherently good notch toughness. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive, shear, and bend strength as well as fracture...