Alloy Digest (1978) 27 (12): SA-352.
Published: 01 December 1978
... USS Dual Phase 80 is a high-strength steel sheet which has a dual phase structure of martensite and ferrite. It provides all the benefits of higher strength with little sacrifice in ductility, formability or weldability. Dual Phase 80 gains strength as it is formed through rapid work hardening...