Alloy Digest (1972) 21 (2): SA-271.
Published: 01 February 1972
... USS COR-TEN C is an atmospheric corrosion-resistant steel with a minimum yield point of 60,000 psi in plates and bars in thicknesses through 1-inch and in shapes having web thicknesses through 3/4 inch. It is suitable for many structural applications. This datasheet provides information...
Journal Articles
Alloy Digest (1972) 21 (7): SA-277.
Published: 01 July 1972
... USS COR-TEN B is an atmospheric corrosion-resistant steel with a minimum yield point of 50,000 psi in plates, bars and structural shapes through 4-in. thick. It is suited for many structural applications. This datasheet provides information on composition, physical properties, elasticity, tensile...
Journal Articles
Alloy Digest (1972) 21 (11): SA-283.
Published: 01 November 1972
... USS COR-TEN A, the original COR-TEN Steel composition (see U.S.S. COR-TEN, Alloy Digest SA-17, April 1954), has 5 to 8 times the atmospheric corrosion resistance of structural carbon steel and a minimum yield point of 50,000 psi in sections through 1/2-inch thick. This datasheet provides...
Journal Articles
Alloy Digest (1954) 3 (4): SA-17.
Published: 01 April 1954
... treatability joinability machinability physical properties shear strength tensile properties U.S.S. COR-TEN weldability workability - DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: SA-17 Steel Alloy APRIL, 1954 U. S. S. COR-TEN (High-Strength Low-Alloy Steel) USS. COR-TEN is a corrosion resistant...