Skip Nav Destination
Close Modal
Search Results for
USS COR-TEN A
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-4 of 4 Search Results for
USS COR-TEN A
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1972) 21 (11): SA-283.
Published: 01 November 1972
... USS COR-TEN A, the original COR-TEN Steel composition (see U.S.S. COR-TEN, Alloy Digest SA-17, April 1954), has 5 to 8 times the atmospheric corrosion resistance of structural carbon steel and a minimum yield point of 50,000 psi in sections through 1/2-inch thick. This datasheet provides...
Abstract
View article
PDF
USS COR-TEN A, the original COR-TEN Steel composition (see U.S.S. COR-TEN, Alloy Digest SA-17, April 1954), has 5 to 8 times the atmospheric corrosion resistance of structural carbon steel and a minimum yield point of 50,000 psi in sections through 1/2-inch thick. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-283. Producer or source: United States Steel Corporation.
Journal Articles
Alloy Digest (1954) 3 (4): SA-17.
Published: 01 April 1954
... treatability joinability machinability physical properties shear strength tensile properties U.S.S. COR-TEN weldability workability - DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: SA-17 Steel Alloy APRIL, 1954 U. S. S. COR-TEN (High-Strength Low-Alloy Steel) USS. COR-TEN is a corrosion resistant...
Abstract
View article
PDF
U.S.S. COR-TEN is a corrosion resistant high-strength steel of low alloy content, intended primarily for weight reduction, or longer life, by means of greater strength and enhanced atmospheric corrosion resistance in applications involving fabrication by forming and welding. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-17. Producer or source: United States Steel Corporation.
Journal Articles
Alloy Digest (1972) 21 (2): SA-271.
Published: 01 February 1972
... USS COR-TEN C is an atmospheric corrosion-resistant steel with a minimum yield point of 60,000 psi in plates and bars in thicknesses through 1-inch and in shapes having web thicknesses through 3/4 inch. It is suitable for many structural applications. This datasheet provides information...
Abstract
View article
PDF
USS COR-TEN C is an atmospheric corrosion-resistant steel with a minimum yield point of 60,000 psi in plates and bars in thicknesses through 1-inch and in shapes having web thicknesses through 3/4 inch. It is suitable for many structural applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-271. Producer or source: United States Steel Corporation.
Journal Articles
Alloy Digest (1972) 21 (7): SA-277.
Published: 01 July 1972
... USS COR-TEN B is an atmospheric corrosion-resistant steel with a minimum yield point of 50,000 psi in plates, bars and structural shapes through 4-in. thick. It is suited for many structural applications. This datasheet provides information on composition, physical properties, elasticity, tensile...
Abstract
View article
PDF
USS COR-TEN B is an atmospheric corrosion-resistant steel with a minimum yield point of 50,000 psi in plates, bars and structural shapes through 4-in. thick. It is suited for many structural applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-277. Producer or source: United States Steel Corporation.