1-3 of 3 Search Results for

USS AR 360

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1977) 26 (5): SA-332.
Published: 01 May 1977
... USS AR 360 is a quenched-and-tempered low-alloy steel designed to fit a broad range of applications where resistance to abrasion is a major consideration. It is used to produce components for mining and materials handling equipment and agricultural implements. This datasheet provides information...
Journal Articles
Alloy Digest (1977) 26 (1): CS-65.
Published: 01 January 1977
... 0.284 0.116 0.124 360 354 6.4 x 10-6 6.6 x 104 6.9 x 104 15.9 21.9 28-30 x 106 Heat Treatment: USS AR300 and AR.350 are supplied in the water quenched-and-tempered condition to provide uniform hardness. The austenitizing temperature is approximately 1625-l 6750F and the tempering temperature is approx...
Journal Articles
Alloy Digest (1970) 19 (12): CS-38.
Published: 01 December 1970
...-hydrogen electrodes and in removing moisture from plate surfaces prior to welding. Corrosion Resistance: LUKENS AR-350 has atmospheric corrosion resistance at least twice that of carbon steel to which no copper has been added. Specification Equivalent: USS AR-350. General Characteristics: LUKENS AR-350...