Alloy Digest (1994) 43 (6): SS-568.
Published: 01 June 1994
... URANUS SB 8 is a super austenitic chromium nickel molybdenum and nitrogen alloy, 25.25.5 Cu type. This grade has been designed for high chloride environments. It is perfectly adapted to pulp and paper medias, stagnant sea water environments and for fabrications handling contaminated phosphoric...