Alloy Digest (1999) 48 (7): SS-751.
Published: 01 July 1999
... URANUS S1 is the development of 15 years research into alloys containing high silicon contents (4% here) to resist the transpassive intergranular corrosion from such chemicals as concentrated nitric acid. This datasheet provides information on composition, physical properties, elasticity, tensile...