Skip Nav Destination
Close Modal
Search Results for
URANUS B6N
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
URANUS B6N
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (7): SS-747.
Published: 01 July 1999
... URANUS B6N is a multipurpose austenitic stainless steel with excellent corrosion properties. This alloy, developed more than 40 years ago, has been improved by the higher addition of nitrogen to approx. 0.13% to increase its structure stability and corrosion resistance. See also URANUS B66, Alloy...
Abstract
View article
PDF
URANUS B6N is a multipurpose austenitic stainless steel with excellent corrosion properties. This alloy, developed more than 40 years ago, has been improved by the higher addition of nitrogen to approx. 0.13% to increase its structure stability and corrosion resistance. See also URANUS B66, Alloy Digest SS-602, July 1995. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as machining and joining. Filing Code: SS-747. Producer or source: Creusot-Marrel. Originally published June 1999, corrected July 1999.