Alloy Digest (1995) 44 (7): SS-602.
Published: 01 July 1995
... URANUS B66 is a high strength super austenitic stainless steel with a pitting resistance equivalent number equal or greater than 50. Applications involve resisting sea water or acid chloride environments. This datasheet provides information on composition, physical properties, elasticity, tensile...
Journal Articles
Alloy Digest (1999) 48 (7): SS-747.
Published: 01 July 1999
... URANUS B6N is a multipurpose austenitic stainless steel with excellent corrosion properties. This alloy, developed more than 40 years ago, has been improved by the higher addition of nitrogen to approx. 0.13% to increase its structure stability and corrosion resistance. See also URANUS B66, Alloy...
Journal Articles
Alloy Digest (2003) 52 (2): Ni-602.
Published: 01 February 2003
... 2.4697 (G-NiCr20Mo15) (cast) Proprietary Hastelloy alloy C22 (Haynes) Proprietary Nicrofer 5621hMoW (Krupp VDM) Superaustenitics ASTM/UNS S32654, S31254, S34565 Proprietary 654SMO (Avesta Polarit) Proprietary Uranus B66 (Usinor Industeel) HAS 59 may be used for dissimilar joints between any combination...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-596.
Published: 01 December 2002
... (Haynes) + Cu Alloy C22 and similar N06022, A 494 Grade CX2MW (cast) 2.4602 (NiCr21Mo14W), Hastelloy Alloy C22 (Haynes), Nicrofer 5621hMoW (Krupp VDM) 2.4697 (G-NiCr20Mo15) (cast) Superaustenitics S32654, S31254, S34565 654SMO (AvestaPolarit), Uranus B66 (Usinor Industeel) Dissimilar joints between any...