Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (10): SS-655.
Published: 01 October 1996
... Uranus 800 HT is a variant of a high chromium and nickel austenitic alloy that combines good corrosion and creep resistance. The alloy is solution annealed to produce a large grain size and remains stable, not being embrittled by the precipitation of sigma phase. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (6): SS-646.
Published: 01 June 1996
... Uranus 800 is employed at temperatures below 600 deg C (1112 deg F) and is the aqueous corrosion-resistant variant of Uranus 800 H and Uranus 800 HT. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes...