... Uranus 45N (UR 45N) is a nitrogen alloyed (>0.15%) austenitic-ferritic stainless steel (2205 type) with improved structural stability and high general, localized, and stress-corrosion resistance properties. The Pitting Resistance Equivalent Number (PREN) is >33. This datasheet provides...
Journal Articles
Alloy Digest (2000) 49 (9): SS-802.
Published: 01 September 2000
... Uranus 45N+ (UR 45N+) is a modification of the 2205 or UNS S31803 composition to which molybdenum and nitrogen have been optimized to develop a pitting resistance equivalent nitrogen (PREN) number that is 36 or greater. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1999) 48 (7): SS-747.
Published: 01 July 1999
... Resistance: General Corrosion. In sulfuric acid environments, the range of concen- trations and temperatures in which UR B6 can be used is much wider than those of most of the other highly corrosion-resistant grades (i.e., 317L (CLI 17.12.3) or 22 Cr Duplex (S 31803 CLI UR 45N General corrosion resistance...