Alloy Digest (2015) 64 (3): SS-1204.
Published: 01 March 2015
... Uranus UR 2202 is considered a lean duplex austenitic/ferritic stainless steel designed to match the corrosion resistance of AISI Type 304L. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture...
Journal Articles
Alloy Digest (2009) 58 (4): SS-1033.
Published: 01 April 2009
... UR 2202 is a lean duplex stainless steel designed to match the corrosion resistance of Type 304SS. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion...