Alloy Digest (2020) 69 (4): Co-130.
Published: 01 April 2020
... UPM Nickel Alloy 188 (UNS R30188 / Werkstoff Number 2.4683) is a low-carbon, cobalt-nickel-chromium-tungsten alloy that combines excellent high-temperature strength with very good oxidation resistance up to 1095 °C (2000 °F). It is widely used in commercial and military aircraft gas turbine...