Alloy Digest (2013) 62 (2): SS-1135.
Published: 01 February 2013
... fabricability of this alloy, combined with its basic corrosion resistance and economy have significantly broadened the utility of ATI 409HP stainless steel. ATI 409HP consists of four grades: UNS S40900, S40910, S40920, and S40930. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2007) 56 (4): SS-990.
Published: 01 April 2007
... hardness joinability physical properties tensile properties workability high-temperature alloys UNS UNS S40920 Chemical Composition, wt. %: (Typical) ASTM A 240, AK Steel 409 UNS S40920 Ultra Form Carbon 0.03 max 0.02 max Manganese 1.00 max 075 max Phosphorus 0.040 max 0.040 max Sulfur 0.010 max...