Journal Articles
Alloy Digest (2020) 69 (9): TS-800.
Published: 01 September 2020
.... Producer or Source: Carpenter Technology Corporation Copyright ┬ę ASM International┬« 2020 2020 ASM International CarTech L6 chemical composition elasticity hardness heat treatability impact toughness machinability physical properties workability UNS T61206 CARTECH L6 (High-Carbon...
Journal Articles
Alloy Digest (2007) 56 (11): TS-657.
Published: 01 November 2007
... TLS L6 wear resistance workability thermal properties UNS T61206 Chemical Composition, wt (Typical Analysis) Carbon 0.70 Manganese 0.60 Silicon 0.25 Chromium 0.70 Nickel 1.40 Iron bal Physical Properties: Density, kg/m3 (lb/in.3) 7861 (0.284) Specific gravity 7.86 Coefficient of linear thermal...
Journal Articles
Alloy Digest (1981) 30 (1): TS-375.
Published: 01 January 1981
... elasticity hardness heat treatability machinability physical properties pinions punches shear blades wear resistance workability UNS T61206 CYCLOPS 16 Filing Code: TS-375 Tool Steel JANUARY 1981 - DATA ON WORLD WIDE METALS AND ALLOYS Q Copyriph? 1960, En9inaaring Pubtications. Inc. MI rights...
Journal Articles
Alloy Digest (1984) 33 (6): TS-423.
Published: 01 June 1984
... chemical composition dies elasticity fracture toughness hardness heat treatability machinability NDS physical properties punches tensile properties wear resistance workability UNS T61206 - DATA ON WORLD WIDE METALS AND AU Filing Code: TB-423 Tool Steel I JUNE 1984 toys @ Copyright 1980...