Alloy Digest (1985) 34 (4): TS-439.
Published: 01 April 1985
... UNS No. T30407 is a high-carbon chromium cold-work tool steel containing vanadium (4.0%) and molybdenum (1.0%). Its carbon and vanadium form a vanadium carbide that provides war resistance many times greater than that of UNS No. T30403 (AISI Type D3). UNS No. T30407 was developed for applications...
Journal Articles
Alloy Digest (1980) 29 (4): TS-361.
Published: 01 April 1980
... punches slitter knives UNS T30407 Filing Coda: TS-361 1 Tool steel O8 MITER1 D-7 APRIL 1666 IMGSSt - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980, Engiwring Publicatiom, Inc. WI rights res~~cd. hblbhai by w-&g&v~f=& Inc. Upper Montclair, New Jersey GUTERL D-7 (Cold-Work Tool Steel; AISI...
Journal Articles
Alloy Digest (1980) 29 (10): TS-371.
Published: 01 October 1980
... dies elasticity hardness heat treatability machinability physical properties pottery tools wear resistance workability UNS T30407 AISI Type D7 Filing Code: Tool Steel TS-371 OCTOBER 1980 - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980. Engineering Publications, Inc. Ail rights...