Alloy Digest (2020) 69 (1): SS-1314.
Published: 01 January 2020
... treatment. For Annealing see Table 3. Table 1 Physical properties Property Unit At Type 430 (UNS S43000) Type 434 (UNS S43400) Type 435 Mod (UNS S44500) Type 436 (UNS S43600) Melting range °C (°F) 1425 1510 (2600 2750) 1425 1510 (2600 2750) 1425 1510 (2600 2750) Density kg/m3 (lb/in.3) 20 °C (68 °F) 7700...
Journal Articles
Alloy Digest (2011) 60 (7): SS-1095.
Published: 01 July 2011
... © ASM International® 2011 2011 ASM International ARCELORMITTAL K45 chemical composition corrosion-resistant alloys corrosivity elasticity heat treatability joinability oxidation resistance physical properties workability thermal properties UNS S44500 DATA ON WORLDWIDE METALS...