Alloy Digest (2020) 69 (7): SS-1322.
Published: 01 July 2020
... Sandmeyer 410S (UNS S41008) is a 13% chromium, ferritic stainless steel. It is a low carbon, non-hardening modification of Type 410 stainless steel. This non-hardening characteristic helps prevent cracking when the alloy is exposed to high temperatures or welded. This datasheet provides...
Journal Articles
Alloy Digest (2006) 55 (5): SS-964.
Published: 01 May 2006
... composition corrosion-resistant alloys elasticity hardness heat treatability joinability oxidation resistance physical properties tensile properties workability thermal properties UNS S41008 Chemical Composition, wt Carbon 0.08 max Manganese 1.00 max Phosphorus 0.040 max Sulfur 0.030 max Silicon...
Journal Articles
Alloy Digest (2020) 69 (11): SS-1329.
Published: 01 November 2020
... workability UNS S41008 OUTOKUMPU MODA 410S/4000 (13% Cr, Ferritic Stainless Steel) Filing Code: SS-1329 Stainless Steel :: November 2020 :: :: :: ::Materials Park, Ohio 44073-0002 440.338.5151 Fax 440.338.4634 www.asminternational.org MemberServiceCenter@asminternational.org ::Published by ASM...
Journal Articles
Alloy Digest (2002) 51 (4): SS-848.
Published: 01 April 2002
... properties tensile properties workability thermal properties UNS S41008 Chemical Composition, wt Carbon 0.08 max Chromium 12.0 14.0 Iron Balance Special arrangements can be made with the producer for compo- sitions within the specified limits depending on the properties required. Physical Properties...
Journal Articles
Alloy Digest (2002) 51 (6): SS-856.
Published: 01 June 2002
... properties tensile properties workability thermal properties UNS S41008 Chemical Composition, wt Carbon 0.08 max Chromium 12.0 14.0 Aluminum 0.10 0.30 Iron bal Physical Properties: Density, kg/m3 (lb/in.3 ) 7700 (0.28) Thermal conductivity, 30 (17) 20 °C (68 °F), W/m K (Btu/(ft h °F)) Specific...
Journal Articles
Alloy Digest (2006) 55 (4): SS-961.
Published: 01 April 2006
... treatability joinability physical properties RA410 RA410S tensile properties workability thermal properties UNS S41000, S41008 RA410 RA410S Chromium 11.50 13.50 11.50 13.50 Carbon 0.15 max 0.08 max Manganese 1.00 max 1.00 max Silicon 1.00 max 1.00 max Nickel 0.75 max 0.60 max...