Alloy Digest (1994) 43 (7): SS-570.
Published: 01 July 1994
... joinability physical properties SUMITOMO DP3 tensile properties wrought stainless steel thermal properties UNS S39226 S31260 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS SUMITOMO DP3 Filing Code: ss-570 Stainless Steel JULY 1994 SUMITOMO DP3 Pdshedby: Alloy Digest. Inc. 1201677.9161 27 Canfiild...