Journal Articles
Alloy Digest (2021) 70 (2): SS-1331.
Published: 01 February 2021
... 2021 ASM International ATI 20-25+Nb chemical composition physical properties elasticity tensile properties creep properties high-temperature alloys workability heat treatability machinability joinability UNS S35140 Producer or Source: ATI ATI 20-25+Nb (26Ni-21Cr-2Mn-1.5Mo-0.5Nb...