Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (10): SS-1310.
Published: 01 October 2019
... or source: Nippon Steel. Producer or Source: Nippon Steel Copyright ┬ę ASM International┬« 2019 2019 ASM International acid resistance chemical composition creep properties high-temperature alloys NSSMC Advanced 347AP physical properties UNS S34752 NSSMC Advanced 347AP is an austenitic...