Skip Nav Destination
Close Modal
Search Results for
UNS S32760
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-7 of 7 Search Results for
UNS S32760
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (3): SS-1140.
Published: 01 March 2013
... toughness hardness heat treatability high-temperature alloys joinability NAS 75N physical properties tensile properties workability thermal properties UNS S32760 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2013, ASM International®. All rights reserved. Data shown are typical, not to be used...
Abstract
View article
PDF
NAS 75N is a super duplex stainless steel with a very high PRE number. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1140. Producer or source: Nippon Yakin Kogyo Company Ltd.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (4): SS-1119.
Published: 01 April 2012
... properties UNS S32760 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2012, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter...
Abstract
View article
PDF
Böhler (or Boehler) A911 is a super duplex ferritic-austenitic chromium-nickel-molybdenum stainless steel with excellent resistance to stress-corrosion cracking, pitting, and crevice corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-1119. Producer or source: Böhler-Uddeholm Specialty Metals Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2017) 66 (9): SS-1269.
Published: 01 September 2017
... 2017 2017 ASM International chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability Outokumpu Forta SDX 100 physical properties tensile properties workability thermal properties UNS S32760 Forta SDX 100 is a super duplex stainless...
Abstract
View article
PDF
Forta SDX 100 is a super duplex stainless with molybdenum, tungsten, and high mechanical properties. It is designed for demanding applications for both corrosion resistance and strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1269. Producer or source: Outokumpu Stainless AB, Avesta Research Centre.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (2): SS-1202.
Published: 01 February 2015
... International® 2015 2015 ASM International chemical composition corrosion-resistant alloys elasticity heat treatability joinability offshore applications physical properties shear strength tensile properties URANUS 2507W workability thermal properties UNS S32760 The high chromium...
Abstract
View article
PDF
The high chromium, molybdenum, and nitrogen contents of alloy UR 2507W (PREN ≥ 40) explain why the grade is very resistant to localized corrosion even in acidified oxidizing environments. The alloy has been used for offshore applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1202. Producer or source: Industeel USA, LLC.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (1): SS-1028.
Published: 01 January 2009
... workability UNS S32760 URANUS® 76N (Super Duplex Austenitic/Ferritic Stainless Steel) The high chromium, molybdenum, and nitrogen contents of alloy UR 76N (PREN 40) explains why the duplex austenitic/ferritic stainless grade is very resistant to localized corrosion. The alloy has been used for offshore...
Abstract
View article
PDF
URANUS 76N contains high chromium, molybdenum, and nitrogen contents and has a pitting resistance equivalent number (PREN) ≥ 40. These factors explain why the duplex austenitic/ferritic stainless grade is very resistant to localized corrosion. The alloy has been used for offshore applications. This datasheet provides information on composition, physical properties, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1028. Producer or source: Industeel USA, LLC.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (5): SS-785.
Published: 01 May 2000
... chemical composition corrosion-resistant alloys DMV 25.7 N elasticity hardness heat treatability high-temperature alloys joinability machinability physical properties tensile properties workability thermal properties UNS S32760 DMV 25.7 N (Duplex Austenitic/Ferritic Stainless Steel) DMV...
Abstract
View article
PDF
DMV 25.7 N is a superferritic-austenitic grade with high mechanical properties and superior corrosion resistance to chlorides, freshwater, and high pressures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-785. Producer or source: DMV Stainless USA Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (11): SS-555.
Published: 01 November 1993
... properties ZERON 100 UNS S32760 Filing Code: ss-555 Stainless Steel I 1 DATA ON WORLD WIDE METALS AND ALLOYS NOVEMBER 1993 CCopvrishr 1993. Atby L3@est. Inc. Att ri9ht.s resewed. Data shown am t*zd, not to be wed for spschmon (r /ma/ &sign. ZERON 100 Published by: Alloy Digesl. Inc. /201-W/-9161 27...
Abstract
View article
PDF
ZERON 100 is a super duplex stainless steel which is manufactured to give a guaranteed corrosion performance by using an equation to control the chemistry in those elements which will determine the corrosion resistance of the material. Major usages in seawater applications, particularly offshore oil gathering systems. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance as well as heat treating, machining, and joining. Filing Code: SS-555. Producer or source: Weir Material Services Ltd.