1-16 of 16

Search Results for UNS S32550

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2008) 57 (4): SS-1010.
Published: 01 April 2008
... Ferralium 255-3SF is an austenitic/ferritic duplex stainless steel equivalent to UNS S32550 as a forged product in bars, discs, and blocks. See also Ferralium 255, Alloy Digest SS-481, January 1987. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2013) 62 (1): SS-1133.
Published: 01 January 2013
... properties tensile properties workability thermal properties UNS S32550 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2013, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH 44073...
Journal Articles
Alloy Digest (2014) 63 (7): SS-1179.
Published: 01 July 2014
... International® 2014 2014 ASM International chemical composition corrosion-resistant alloys elasticity ELECTRALLOY ALLOY EC25540 fracture toughness hardness heat treatability joinability machinability physical properties tensile properties workability thermal properties UNS S32550 DATA...
Journal Articles
Alloy Digest (2009) 58 (8): SS-1041.
Published: 01 August 2009
... machinability physical properties tensile properties workability thermal properties UNS S32550 FERRINOX® 255 (Ferritic/Austenitic Duplex Stainless Steel) Ferrinox 255 is categorized as a super duplex (austenitic/ferritic) stainless steel. This high-performance alloy combines high mechanical strengths...
Journal Articles
Alloy Digest (1988) 37 (5): SS-495.
Published: 01 May 1988
... 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity fracture toughness hardness heat treatability joinability JS ALLOY 255 machinability physical properties tensile properties workability UNS S32550 JS ALLOY 255 Filing Code: SS-495 Stainless...
Journal Articles
Alloy Digest (2008) 57 (2): SS-1007.
Published: 01 February 2008
... properties workability wrought stainless steel thermal properties UNS S32550 Chemical Composition, wt Carbon 0.040 max Chromium 24.0 27.0 Copper 1.50 2.50 Molybdenum 2.90 3.90 Manganese 1.50 max Nitrogen 0.10 0.25 Nickel 4.50 6.50 Phosphorus 0.040 max Sulfur 0.030 max Silicon 1.00 max Iron bal...
Journal Articles
Alloy Digest (2002) 51 (6): SS-786.
Published: 01 June 2002
... joinability machinability physical properties tensile properties workability thermal properties UNS S32550 ALLEGHENY LUDLUM ALLOY 255 (Duplex Austenitic-Ferritic Stainless Steel) Allegheny Ludlum alloy 255 is a high-strength duplex stainless steel. It combines high mechanical strength, ductility...
Journal Articles
Alloy Digest (1995) 44 (9): SS-611.
Published: 01 September 1995
... material are shown in Figure 2. The properties for bar and forging are those quoted in UNS S32550 with the exception of elongation, which for alloy SD40 is 10% higher than for the UNS designation. Hardness, which is limited to 270 HB compared with 297 for the ASTM speciti- cation and notch impact for which...
Journal Articles
Alloy Digest (1995) 44 (8): SS-606.
Published: 01 August 1995
... International cast metal products chemical composition FERRALIUM 255-3SC fracture toughness hardness heat treatability high-temperature alloys joinability machinability physical properties tensile properties workability thermal properties UNS S32550 Filing Code: Stainless Steel ss-505...
Journal Articles
Alloy Digest (1994) 43 (5): SS-566.
Published: 01 May 1994
...: Creusot-Marrel Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys heat treatability high-temperature alloys joinability physical properties tensile properties URANUS 52N workability thermal properties UNS S32550 fJy p&&q Etl...
Journal Articles
Alloy Digest (1995) 44 (4): SS-592.
Published: 01 April 1995
... are to be avoided. Typical temperature range of use: -50 C/+27OC (-58F/+518F) cRmcALPrmNGlifMPfmnlREoNmLDED~~ GRADE PIUFR coRRosK)wcarEr6A:.1oal#wEIonTu)fs OR= US Specification Equivalents: EURONORM 1.4507 - X2 Cr Ni MO Cu N 25.6.3 AFNOR .23 CNDU 25.07 AZ DIN W.Nr 1.4507 A.S.T.M. UNS S32550 in A240 Products...
Journal Articles
Alloy Digest (2007) 56 (8): SS-995.
Published: 01 August 2007
... S32550 (wrought) ASTM A 351 and A 744 grade CD4MCu(N) ASTM A890 grade 1A, UNS J93370 ASTM A 890 grade 1B, UNS J93372 BS 3100, grade 332C13 BS 3146, grade ANC21 DIN 1.4515, G-X3CrNiMoCuN 26 6 3 DIN 1.4517, G-X3CrNiMoCuN 26 6 3 3 Proprietary alloys Ferralium 255 and SD40 (Meighs); Uranus 50M, 55, 52N, 52N...
Journal Articles
Alloy Digest (2005) 54 (9): Cu-736.
Published: 01 September 2005
... 0.125 roughing Turning, 150 300 500 1000 0.15 0.4 0.006 0.015 0.5 0.02 finishing Tips Carbide tipped using water-soluble lubricant Table 3 Alloy Comparisons Yield strength, 0.2% Hydrogen Antigalling behavior Alloy MPa ksi embrittlement resistance Biofouling resistance UNS S32550 720 104 Can...
Journal Articles
Alloy Digest (2018) 67 (12): SS-1299.
Published: 01 December 2018
... duplex stainless steel. Hot isostatic pressed components have isotropic properties, meaning the mechanical properties are similar in all directions. The chemical composition is optimized for manufacturing large components with high wall thickness and is very similar to ASTM A182-F61 (UNS S32550), which...
Journal Articles
Alloy Digest (1987) 36 (1): SS-481.
Published: 01 January 1987
... to stress-corrosioncracking in sodtum chlortdc. seawater and many oiher emironments The manuiacturers can furnish a large amount of data on corroston Crevices Maximum rcststancc in Larious media under a variety of conditions. Initiated* Depth of Specification Equivalents: .4lloy 9 Attack. mm UNS No. S32550...
Journal Articles
Alloy Digest (2006) 55 (2): Cu-740.
Published: 01 February 2006
... rate Alloy MPa ksi MPa ksi in fresh water, mm3/h . m circular-mil/ft W/m . K Btu/(ft . h . °F) Hidurax 1 400 58 700 102 0.6 0.17 102 42 24.3 BS 970 070M55 355 51 700 102 >4 1.0 602 13.4 7.7 medium-carbon steel 316 stainless steel 205 30 515 75 1.7 0.75 451 16.2 9.4 S32550 superduplex 550 80 760...