Alloy Digest (2010) 59 (5): SS-1064.
Published: 01 May 2010
... hardness heat treatability joinability machinability NAS 254N physical properties tensile properties workability UNS S32053 DATA ON WORLDWIDE METALS AND ALLOYS Copyright Ā© 2010, ASM InternationalĀ®. All rights reserved. Data shown are typical, not to be used for specification or final design...