Alloy Digest (2021) 70 (5): SS-1335.
Published: 01 May 2021
... ATI 2003 (UNS S32003) is a molybdenum-enhanced lean duplex stainless steel (LDSS) that was developed to fill the performance gap between type 316L (UNS S31603) and 2205 duplex (UNS S32205) stainless steels. ATI 2003 has reduced alloy content, which makes it less costly than 2205 duplex, yet ATI...
Journal Articles
Alloy Digest (2017) 66 (2): SS-1258.
Published: 01 February 2017
.... Copyright © ASM International® 2017 2017 ASM International ATI 2003 chemical composition corrosion-resistant alloys elasticity fatigue properties hardness heat treatability joinability physical properties tensile properties workability UNS S32003 ATI 2003 lean duplex stainless steel...