Alloy Digest (2002) 51 (12): SS-869.
Published: 01 December 2002
... treatability high-temperature alloys joinability microstructure physical properties tensile properties workability thermal properties UNS S32002 Chemical Composition, wt Carbon 0.030 max Manganese 2.0 max Phosphorus 0.030 max Sulfur 0.020 max Silicon 1.0 max Chromium 19.5 22.5 Nickel 3.0 4.0...