Alloy Digest (1989) 38 (1): SS-502.
Published: 01 January 1989
... Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity hardness heat treatability JESSOP TYPE 317L JESSOP TYPE 317L PLUS joinability machinability physical properties tensile properties workability UNS S31703...
Journal Articles
Alloy Digest (1993) 42 (4): SS-542.
Published: 01 April 1993
... treatability joinability physical properties tensile properties workability thermal properties UNS S31703 S31725 S31726 RdMl ri ALLEGHENY LUDLUM TYPE ei&e~ ss-542 31 7LXNTM, 31 7LXTM, AND 317L 1 APRIL 1993 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS CQDjT@[email protected]@htSMBWV6d. P...
Journal Articles
Alloy Digest (2002) 51 (3): SS-846.
Published: 01 March 2002
... Composition, wt (Nominal) 317L 317L 4 317L 4N (UNS S31703) (UNS S31725) (UNS S31726) Carbon 0.030 max 0.030 max 0.030 max Manganese 2.00 max 2.00 max 2.00 max Phosphorus 0.045 max 0.045 max 0.045 max Silicon 0.75 max 0.75 max 0.75 max Sulfur 0.030 max 0.030 max 0.030 max Chromium 18.0 20.0 18.0 20.0 17.0 20.0...