Sort by
Journal Articles
Alloy Digest (2019) 68 (8): SS-1308.
Published: 01 August 2019
... resistance workability thermal properties UNS S31675 Sandvik High-N is both N and Mo alloyed austenitic stainless steel. Chemical Composition, wt.% (Nominal) Carbon 0.06 max Silicon 0.60 max Manganese 4.0 Phosphorus 0.025 max Sulfur 0.003 max Chromium 20.5 Nickel 9.5 Molybdenum 2.4 Copper 0.20 max...
Journal Articles
Alloy Digest (2014) 63 (2): SS-1168.
Published: 01 February 2014
... physical properties SANDVIK SANRIG 80 tensile strength workability UNS S31675 DATA ON WORLDWIDE METALS AND ALLOYS Copyright ┬ę 2014, ASM International┬«. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH...