Alloy Digest (2002) 51 (3): SS-847.
Published: 01 March 2002
... composition corrosion-resistant alloys elasticity heat treatability joinability machinability NIROSTA 4461 physical properties tensile properties workability thermal properties UNS S31643 Chemical Composition, wt Carbon 0.020 max Chromium 17.00 18.5 Nickel 11.5 13.5 Molybdenum 2.0 2.5 Titanium...