Alloy Digest (1999) 48 (7): SS-751.
Published: 01 July 1999
... ASM International chemical composition corrosion-resistant alloys corrosivity elasticity heat treatability high-temperature alloys joinability physical properties shear strength tensile properties URANUS S1 workability thermal properties UNS S30600 URANUS S1 (High-Silicon...
Journal Articles
Alloy Digest (2001) 50 (2): SS-819.
Published: 01 February 2001
... corrosion-resistant alloys hardness joinability physical properties tensile properties UNS S30600 Allegheny Ludlum alloy AL 610 is an austenitic stainless steel alloy with a special composition including high silicon to specifically resist high concentrations of nitric acid. AL is a trademark...