Alloy Digest (1999) 48 (9): SS-763.
Published: 01 September 1999
... machinability marine shafts physical properties power components tensile strength workability thermal properties UNS S30452 CARPENTER STAINLESS TYPE 304HN (High-Temperature Austenitic Stainless Steel) Carpenter Stainless Type 304HN is the high-nitrogen version of Type 304 and 304H stainless steels...
Journal Articles
Alloy Digest (1979) 28 (10): SS-368.
Published: 01 October 1979
... components CARPENTER STAINLESS TYPE 304HN chemical composition corrosion-resistant alloys ductility elasticity hardness heat treatability joinability machinability marine hardware physical properties tensile strength workability UNS S30452 Filing Code: SS-368 CARPENTER STAINLESS TYPE 304HN...