Alloy Digest (2002) 51 (10): SS-864.
Published: 01 October 2002
... thermal properties UNS S30451 Chemical Composition, wt Carbon 0.06 max Chromium 18.0 20.0 Nickel 8.0 11.0 Nitrogen 0.12 0.22 Iron bal Physical Properties: Density, kg/m3 (lb/in.3 ) 7900 (0.285) Thermal conductivity, 20 °C (68 °F), 15 (8.7) W/m K (Btu/(ft h °F)) Specific heat capacity, 20 °C (68...