Alloy Digest (2005) 54 (9): SS-940.
Published: 01 September 2005
... CARPENTER 303 Al MODIFIED chemical composition corrosion-resistant alloys elasticity hardness heat treatability high-temperature alloys joinability machinability physical properties tensile properties workability UNS S30345 Chemical Composition, wt (Type analysis) Carbon 0.15 max Manganese...