1-2 of 2 Search Results for

UNS S21900, S21904

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2018) 67 (11): SS-1297.
Published: 01 November 2018
...® 2018 2018 ASM International chemical composition corrosion-resistant alloys Electralloy Nitronic 40 heat treatability high-temperature alloys joinability low-temperature alloys machinability physical properties tensile properties thermal properties UNS S21900, S21904 Electralloy s...
Journal Articles
Alloy Digest (1990) 39 (8): SS-327.
Published: 01 August 1990
... (Classification E219) ASME Design Allowables (Table UHA-23, Sec. VIII Division 1. UNS S21900 (XMlO) S21904 (KMll). General Characteristics: Armco NITRONIC 40 stainless steel has high strength and good fabricabilityandweldability.Itretainsgoodtoughnessto423 F. It has good elevated temperature poperties and...