Alloy Digest (2001) 50 (7): SS-825.
Published: 01 July 2001
... ALLEGHENY LUDLUM TYPE 201L chemical composition corrosion-resistant alloys corrosivity hardness heat treatability physical properties tensile properties thermal properties UNS S20103 ALLEGHENY LUDLUM TYPE 201L (High Manganese Austenitic Stainless Steel) Type 201L is a low-carbon version of type...