Alloy Digest (1988) 37 (6): SS-496.
Published: 01 June 1988
... alloys joinability machinability physical properties tensile properties workability UNS S15700 AL 15-7 PRECIPITATION Filing Code: SS-496 HARDENING ALLOY Stainless Steel - DATA ON WORLD WIDE METALS AND ALLOYS JUNE 1988 0 Copyri#ht 1998. Alloy DI#CSI. Inc. All rights -cd. Fubluhed by: Alloy hpn...
Journal Articles
Alloy Digest (1989) 38 (10): SS-75.
Published: 01 October 1989
... properties workability UNS S15700 ARMCO PH 15-7 MO Filing Code: ss-75 Stainless Steel REVISED OCTOBER 1989 JUNE 1958 -DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS eapyligM 1969, Nby Dise+t. hc Alilg7llls n*rerwd. Publid& by: Away Digaot. It-c I x)1-677-9161 D.¶faahyIurQpicdmtlobs~hY 27 Cdidd Street...
Journal Articles
Alloy Digest (1997) 46 (8): SS-693.
Published: 01 August 1997
... alloys elasticity hardness heat treatability high-temperature alloys joinability physical properties tensile properties workability thermal properties UNS S15700 c DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: ss-693 d!ER!k Stainless Steel u - August 1997 ARMCO PH 15-7 MO STAINLESS STEEL...