Alloy Digest (2023) 72 (8): Ti-195.
Published: 01 August 2023
... Aubert & Duval Ti17 (UNS R58650) is a “beta-rich” alpha-beta titanium-aluminum-molybdenum-chromium-zirconium-tin alloy. This alloy has higher tensile and creep strengths than Ti-6Al-4V. While its hardenability is similar to that of other beta alloys, Aubert & Duval Ti17 has a lower density...
Journal Articles
Alloy Digest (2013) 62 (6): Ti-150.
Published: 01 June 2013
... compressor discs corrosion-resistant alloys electrical applications fan hardness heat treatability joinability physical properties tensile properties workability UNS R58650 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2013, ASM International®. All rights reserved. Data shown are typical...
Journal Articles
Alloy Digest (2012) 61 (1): Ti-149.
Published: 01 January 2012
... alloys hardness heat treatability joinability physical properties tensile properties workability UNS R58650 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2012, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM...
Journal Articles
Alloy Digest (2001) 50 (8): Ti-117.
Published: 01 August 2001
... fracture toughness hardness high-temperature alloys physical properties RMI 5Al-2Zr-2Sn-4Mo-4Cr (Ti-17) tensile properties thermal properties UNS R58650 Ti-17 alloy is an -rich near- alloy that is sometimes classified as an alloy. Unlike other or near- alloys, Ti-17 offers good creep...
Journal Articles
Alloy Digest (2004) 53 (11): Ti-135.
Published: 01 November 2004
... of its high chromium content. Specification Equivalents: UNS R58650 SAE AMS 4995 billet General Characteristics: This alloy was developed by General Electric as a high-strength deep-hardening alloy for fan and compressor discs and for other large components. It has been classified as a beta-rich alpha...