Alloy Digest (2021) 70 (7): Ti-180.
Published: 01 July 2021
... CarTech Ti 15V-3Cr-3Sn-3Al (UNS R58153) is a metastable beta titanium alloy that offers substantial weight reduction in comparison with other engineering materials. If used in the solution heat treated condition, the alloy has excellent cold formability. In the aged condition, the alloy has high...