Alloy Digest (2021) 70 (1): Ti-174.
Published: 01 January 2021
... machinability joinability UNS R56406 Producer or Source: Arcam AB (a GE Additive company) httpsdoi.org/10.31399/asm.ad.ti0174 Copyright Ā© 2021, ASM InternationalĀ®. All rights reserved. Powder Specification The Arcam Ti6Al4V powder for electron beam melting (EBM) is produced using the proprietary plasma...