Alloy Digest (2021) 70 (2): Ti-175.
Published: 01 February 2021
... International ATI CP Grade 7 Titanium chemical composition physical properties elasticity tensile properties bend strength corrosion-resistant alloys workability heat treatability joinability UNS R52400 ATI CP Grade 7 Titanium (Ti-0.2Pd Alloy) Filing Code: Ti-175 Titanium :: February 2021...
Journal Articles
Alloy Digest (2020) 69 (1): Ti-162.
Published: 01 January 2020
... Composition, wt%, for indicated grade (UNS designation)(a) 1 (R50250) 2 (R50400) 3 (R50550) 4 (R50700) 7 (R52400) 11 (R52250) 16 (R52402) 17 (R52252) Nitrogen 0.03 0.03 0.05 0.05 0.03 0.03 0.03 0.03 Carbon 0.08 0.08 0.08 0.08 0.08 0.08 0.08 0.08 Hydrogen 0.015 0.015 0.015 0.015 0.015 0.015 0.015 0.015 Iron...