Alloy Digest (2021) 70 (1): Co-132.
Published: 01 January 2021
... Additive company). Copyright © ASM International® 2021 2021 ASM International Arcam ASTM F75 CoCr chemical composition physical properties microstructure hardness tensile properties fatigue properties corrosion-resistant alloys heat treatability machinability UNS R30075 Producer or...