Alloy Digest (1985) 34 (2): Ag-11.
Published: 01 February 1985
... conductivity workability UNS P07931 P07932 1 Sterling Silver Filing Code: Ag-11 Silver Alloy Or FEBRUARY 1985 BICBST - DATA ON WORLD WIDE METALS AND ALLOYS - Puhlishrtl ht @ Copyright 1980. Engineering Publications. Inc. Ail rights reserved. ISSN: 002-614X Alloy Digest. Inc. 27 Canfield Smeet Orange. New...